DESCRIPTION
Reddish, brown (or sometimes black) stains appearing as blotches or streaks on surface or paint. See also Tannin Staining.
POSSIBLE CAUSE
Steel in contact with air and moisture will rust (e.g., nails, steel railings, damaged galvanized, flashing, etc.).
Steel nails may develop black discoloration when in contact with damp wood that possesses a high amount of tannic acid.
SOLUTION
Prime bare steel as soon as possible with a rust-inhibiting primer or finish.
Replace steel nails with galvanized or other non-rusting nails.
Rusted nails that cannot be removed must be sanded to shiny metal; countersunk; coated with a rust-preventive primer; and then caulked, filled, or patched; and topcoated.
INTERIOR
PRIMER
(if needed)
All Surface Enamel Primer
DTM Primer/Finish
Pro Industrial™ ProCryl® Primer
or reapply the same coating
SUGGESTED FINISH
Emerald®
Duration Home®
Cashmere®
SuperPaint®
ProClassic®
All Surface Enamel
EXTERIOR
PRIMER
(if needed)
Exterior Oil-Based Wood Primer
All Surface Enamel Primer
DTM Primer/Finish
Pro Industrial™ ProCryl® Primer
SUGGESTED FINISH
Emerald®
Duration®
Resilienceâ„¢
SuperPaint®
A-100®
WoodScapes®
or reapply the same coating