DESCRIPTION

Deep, irregular cracks resembling dried mud in the dry paint film.

POSSIBLE CAUSE


  • Paint is applied too thick.
     

  • Paint is allowed to build up in corners during application.
     

  • Surface was not prepared properly; contaminants were not removed.

SOLUTION

See Lead Information.
 

  • Follow label and data page directions for the appropriate surface preparation.
     

  • Follow label and data page directions for the appropriate film build.
     

  • Determine the correct roller cover based on the coating being applied and the surface. On smooth surfaces, a mohair, 1/4", or 3/8" roller nap is usually sufficient. On textured surfaces, a 3/4" nap or greater is needed.
     

  • Smooth the coating by scraping and/or sanding, prime if needed, and repaint.
     

  • Quality paints have very good application and hiding properties, which minimize the tendency to apply too thick a coat of paint.


INTERIOR

EXTERIOR

App Server Details

generated on: Sun Dec 22 08:08:20 UTC 2024

Host: tsapp-688b49ccb7-qblg9

Server Port: 443

Local Port: 5443

Instance: server1

It took 0 milliseconds to generate this page.