DESCRIPTION

Thin, long, and relatively straight cracks that form in the paint film, usually in the direction of the plywood grain.

POSSIBLE CAUSE

  • Plywood is prone to cracking because of its method of manufacture. Plywood cracks from its expansion and contraction with changing moisture content. Stresses are induced which later show up as cracking. Many small fissures are produced in films of paints and stains that have been applied to insufficiently dry plywood. The edges of these cracks may protrude upward and be felt as sharp burrs. Subsequently, this coating may become detached from the edges of the cracks and lead to flaking.

SOLUTION

See Lead Information.

  • New wood: To prevent cracking of newly installed exterior plywood, sand and immediately prime with Exterior Latex Wood Primer. Even minimal exposure to the elements will cause unprotected plywood to degrade.

  • Repaint: If the cracking is not extensive, clean the surface thoroughly, then sand surface smooth and wipe off dust. The plywood must be thoroughly dry. If cracking is severe, replace the wood.

  • Be sure that edges and joints are sufficiently sealed or caulked to prevent water from getting into the panels.


EXTERIOR

Primer
PrimeRxâ„¢ Peel Bonding Primer
Exterior Latex Wood Primer

Suggested Finish
Emerald®
Duration®
Resilienceâ„¢
SuperPaint®
A-100®
WoodScapes®

See Exterior Paints

App Server Details

generated on: Thu Dec 05 02:20:32 UTC 2024

Host: tsapp-5d57d58ccd-wl4vl

Server Port: 443

Local Port: 5443

Instance: server1

It took 0 milliseconds to generate this page.