Skip navigation

DESCRIPTION

The splitting of a dry paint film through at least one coat. In its early stages, the problem appears as hairline cracks; in its later stages, flaking occurs.

POSSIBLE CAUSE


  • Use of a paint that has lower adhesion and flexibility properties.                    
     

  • Over-thinning or over-spreading the paint.
     

  • Inadequate surface preparation, or applying the paint to bare wood without first applying a primer.
     

  • Excessive hardening and embrittlement of paint as it ages, the coating loses the ability to expand and contract with temperature and humidity changes.

SOLUTION

See Lead Information.
         

  • Remove loose and flaking paint with a scraper or wire brush, sanding the surface and feathering the edges. If the flaking occurs in multiple layers of paint, use of a spackling compound may be necessary to make a uniform surface. Test the coating surrounding any peeled areas out about 6" to 12" to be sure the adhesion is adequate.
     

  • Prime bare wood or plaster before repainting.
     

  • Apply the coatings at the recommended spreading rate (e.g. the recommended total area that can be painted) and using the recommended thinning rate (e.g. the recommended percentage that a coating may be diluted).


INTERIOR

EXTERIOR

App Server Details

generated on: Tue Dec 24 08:00:44 UTC 2024

Host: tsapp-688b49ccb7-7mc9x

Server Port: 443

Local Port: 5443

Instance: server1

It took 0 milliseconds to generate this page.