Skip navigation

 

DESCRIPTION

A rough, crinkled paint surface, which occurs when uncured paint forms a "skin".

POSSIBLE CAUSE

 

  • Paint applied too heavily.
     

  • Painting under extremely hot conditions or cool damp conditions, which causes the paint film to dry faster on top than on the bottom.
     

  • Exposure of uncured paint to rain, dew, fog, or high humidity levels.
     

  • Applying topcoat of paint to insufficiently cured primer or first coat of paint.
     

  • Painting over contaminated surface (e.g., dirt or wax).

 

SOLUTION

See Lead Information.
  • Scrape or sand to remove the wrinkled coating; sand the surface smooth to blend it in to the surrounding coating. Make sure the surface is thoroughly clean.
     

  • If needed, prime bare areas with the appropriate primer, allowing it to dry completely.
     

  • Reapply the coating following the label and data page instructions for spreading rate and environmental conditions.

INTERIOR

EXTERIOR

App Server Details

generated on: Mon Dec 23 08:07:30 UTC 2024

Host: tsapp-688b49ccb7-24rx4

Server Port: 443

Local Port: 5443

Instance: server1

It took 0 milliseconds to generate this page.